Download Article

If you only need to bend wood for a one-time project, laminating the wood is the least labor-intensive option. Steaming the wood to make it flexible gives you stronger curves, but the process requires a fair amount of set up. Finally, kerfing is a quick approach that only requires a saw, but the result is too weak to use in many projects. Whichever approach you use, experiment with spare lumber first while you're learning the ropes.

Method 1

Method 1 of 3:

Laminating

Download Article

  1. 1

    Create a bending form. Set a drawing compass to the thickness of your lumber. Using the compass, trace two lines on a stack of plywood in the shape you'd like to bend your wood. Cut along both lines with a bandsaw. Now you have a gap the perfect size for your lumber, and a two-part plywood form to press the lumber from both sides.[1]

    • Alternatively, just cut one line to create the inner curve, and use clamps to press the lumber against it.
    • There will be a small amount of spring-back after you release the wood with this method. Bend it slightly farther than you want the final shape.
  2. 2

    Plane your lumber into thin strips. Once glued back together, these strips will be much more flexible than the original lumber. You can use any type of wood, but cross-grained wood and wood with knots are likely to break.[2] Plane it into strips according to how far you plan to bend it:[3]

    • For a curve with a 2 to 4 inch radius (5–10 cm), plane the wood into 3/32" (2.4 mm) strips.
    • For a curve with a 4 to 8 inch (10–20 cm) radius, plane to 1/8" (3.2 mm).
    • For an 8 to 12 inch (20–30 cm) radius, plane to 3/16" (4.8 mm).
    • For a radius greater than 12 inches (30 cm), plane to 1/4" (6.4 mm).
    • These are guidelines to use as a starting point. The wood species and grain slope affect the result, so you may need to experiment.

    Advertisem*nt

  3. 3

    Soak the strips in hot water (optional). This will make the wood more flexible, which may be necessary for tight bends. However, for best results, you will need to keep the wood wet for the first three or four hours after you bend it. Skip this step if you prefer a less time-intensive approach, or if you are only creating slight bends.[4]

  4. 4

    Glue the strips together immediately. Working with freshly planed surfaces will increase the strength of the bond. You can use epoxy, polyurethane, aliphatic resin, or just about any high-strength glue that works on wood and meets the needs of your project.[5]

    • Distribute the glue as evenly as possible. Rolling a 3/8" (9.5 mm) threaded rod over the wood can give better results than brushing on the glue.
    • Flip every other strip end-to-end before gluing. This will prevent the grain slope from lining up, removing lines of weakness.
  5. 5

    Clamp the wood onto your bending form. Bend the laminated wood along the piece of plywood you prepared. Clamp it tight in several places. The more clamps you use, the less chance there is that gaps will appear between strips, and the closer your wood will get to the desired shape.

  6. 6

    Leave the wood until the glue sets. Check your glue label instructions for the curing time. (If it doesn't say, wait 24 hours.[6]) After that, the wood should stay in its new shape.

    • If you soaked the wood, don't forget to keep it wet for the first three or four hours.
  7. Advertisem*nt

Method 2

Method 2 of 3:

Steam Bending

Download Article

  1. 1

    Choose your lumber. Green and air-dried hardwood are both suitable for steaming. The risk of breaking is too high for kiln-dried wood, softwood, and any lumber with less than 10% moisture content (15% for tight bends).[7][8] Straight-grained lumber with minimal knots is recommended, but you can use cross-grained lumber with a grain slope less than 1:15.[9]

    • Hackberry and oak are among the best hardwoods for this approach; a 1 inch (2.5 cm) thick piece can bend to a curve radius as tight as 2 inches (5 cm). Maple, cherry, and poplar are prone to damage and only accept slight bends.[10]
  2. 2

    Build a steam box. Construct a tongue-and-groove box large enough to hold your lumber out of ¾" (19 mm) thick, exterior-grade fir plywood. Fit a hinged door on each end, and seal the joints with silicone and screws. Insert brass rods or wooden dowels through the sides for the lumber to rest on, so steam can circulate around it. Leave the box unpainted and unsealed so it can dry out between uses.

    • If you are only steaming parts the size of walking sticks or smaller, you can use a length of ABS pipe with a 2 to 4 inch (5–10 cm) diameter instead.
    • Another alternative is to melt 6 mil polyethylene into a plastic bag around your lumber. You can then bend the lumber while it is still in the steam bag for maximum flexibility.[11]
  3. 3

    Set up steam collection and drainage. You can use an electric tea kettle as a steam source for steaming pieces 1" x 2" (19 x 38 mm) or smaller. For larger pieces, use a clean pressure cooker, metal gas can, or other large container over an electric hot plate; or rent a wallpaper steamer. Connect the steam source to your box as follows:[12]

    • Connect a 1½" (3.8 cm) diameter hose to the steam source with tightly fitted nuts. Cut a hole in the steam source if necessary to accommodate this.
    • Cut a hole in the base of the box and attach the other end of the hose.
    • Drill a few small drainage holes into the base of the box, especially toward one end. Set up the box so it slopes toward this end.
    • Optionally, drill a hole in the top of the box and plug it with a stopper. This allows you to insert a thermometer.
  4. 4

    Build a bending form. Use a bandsaw to cut a stack of plywood into the shape of the inner curve. Screw the plywood onto a table to create a form to bend your wood around once steamed. To prevent the outer curve from splintering, you can either form a similar plywood back (just cut out the thickness of your lumber from the remaining plywood), or secure a metal bending strap to your table. Unless you are only bending a slight curve, you will also need to place clamps against the ends of the lumber.[13]

    • Metal straps may discolor your wood. If this is an issue, use an oversize piece of lumber and remove the affected area.
    • If you will bend the wood to a curve radius less than 4" (10 cm), you will need a stronger material to bend it around. Cut off the tip of the plywood corner and replace it with a piece of hardwood.
  5. 5

    Steam the wood. Put the wood into the box, seal it, and heat plenty of water to create steam. As a general rule, wood needs steaming for one hour per inch (2.5 cm) of thickness at 212ºF (100ºC). Put in a few pieces of test lumber as well so you can experiment, since moisture content, wood species, and other factors all affect the wood's behavior. (For example, if your wood has a moisture content above 20%, you may only need to steam for half an hour per inch.[14])

    • If you have a thermometer, use a small hole at the top of the box to check the temperature. If it's too cool, wrap the box in an insulating material.
    • To avoid steam burns, wear work gloves and keep your face back when opening the steam box.
  6. 6

    Bend the wood onto the form. The heat and moisture from the steam will soften the lignin, a substance responsible for wood's rigid shape. Immediately after steaming, place the wood against one end piece on your bending form. Starting at that end, bend the wood around your form at a moderate, steady pace. Compress the wood securely between the two pieces of plywood (or the plywood and backing strap). If the wood is not secure, the outer edge may stretch and weaken.

    • If the wood cracks, it needs more steaming.
    • If the wood wrinkles along the inner edge, it may have steamed too long, or there may be too much compression.
  7. 7

    Leave the wood to cool and dry. The length of time varies depending on the type of wood, thickness, and intended purpose. As a starting point, keep the wood in a well-ventilated location for 24 hours before removing it from the bending form.[15] If it cooled sufficiently, the lumber should hold its new shape indefinitely.

  8. Advertisem*nt

Method 3

Method 3 of 3:

Kerfing

Download Article

  1. 1

    Plan your project. A kerf is just a saw cut, and kerfing means cutting a series of these slits so your wood can bend. The result is much weaker than other methods of bending wood, but it keeps the wood permanently flexible along that curve. It is also the fastest approach, and does not require special equipment.

  2. 2

    Cut a series of grooves against the grain. The cuts must be against the grain to reduce the chance of splitting the wood. Use a table saw to make these cuts along the part of the wood you'd like to bend. Space your cuts evenly (and close together) with a jig, or use a visual indicator on your table to get a consistent distance between cuts.

  3. 3

    Cut almost to the edge of the wood. In order to bend your wood more than a slight curve, you'll need to cut almost entirely through the wood. Leave only a thin edge to hold the wood together.

  4. 4

    Bend the wood inward. Bend the wood so the "spines" left by your cut touch, forming a single stress-bearing edge. You can now keep the bend in place by fastening the two ends of the lumber to a stable object. Remember that this is a weak bend, and do not rely on it to support much weight or stress.

  5. 5

    Fill the kerfs if desired. If you want to hide the gaps left by the saw, plug them with wood filler that matches your lumber. Alternatively, leave the wood as-is if you prefer the aesthetic, or if you would like to bend it to different angles.

  6. Advertisem*nt

Community Q&A

Search

Add New Question

  • Question

    Can I do this with branches?

    3 Ways to Make Wood Flexible - wikiHow (24)

    Community Answer

    Branches are easiest to bend when they're still living (green inside), but have had a little time off the tree. Soak them in hot water, bend slowly, then clamp in place until dry. For sharp bends, you can steam and bend repeatedly, scraping a little wood off the inner curve to allow for more compression.

    Thanks! We're glad this was helpful.
    Thank you for your feedback.
    As a small thank you, we’d like to offer you a $30 gift card (valid at GoNift.com). Use it to try out great new products and services nationwide without paying full price—wine, food delivery, clothing and more. Enjoy!Claim Your GiftIf wikiHow has helped you, please consider a small contribution to support us in helping more readers like you. We’re committed to providing the world with free how-to resources, and even $1 helps us in our mission.Support wikiHow

    YesNo

    Not Helpful 4Helpful 8

  • Question

    Which wood is most suitable to bend and why?

    3 Ways to Make Wood Flexible - wikiHow (25)

    Community Answer

    Based on experiments, oak (both red and white) and hackberry lumber are probably the best choices for bending into sharp curves. Variation between tree species is complicated, but it likely has something to do with strength, moisture content, and the structure of the "lignin" that holds the tree cells together.

    Thanks! We're glad this was helpful.
    Thank you for your feedback.
    As a small thank you, we’d like to offer you a $30 gift card (valid at GoNift.com). Use it to try out great new products and services nationwide without paying full price—wine, food delivery, clothing and more. Enjoy!Claim Your GiftIf wikiHow has helped you, please consider a small contribution to support us in helping more readers like you. We’re committed to providing the world with free how-to resources, and even $1 helps us in our mission.Support wikiHow

    YesNo

    Not Helpful 3Helpful 9

  • Question

    How do you make a crown of thorns?

    3 Ways to Make Wood Flexible - wikiHow (26)

    Community Answer

    Cut a small, flexible branch off a tree, loop it in a circle, and fasten with florist's wire. Weave more branches around the main loop and fasten with more wire when necessary. If you can't find a tree with thorns, glue on your own thorns using toothpicks or skewers, then stain the whole crown with a dark wood stain.

    Thanks! We're glad this was helpful.
    Thank you for your feedback.
    As a small thank you, we’d like to offer you a $30 gift card (valid at GoNift.com). Use it to try out great new products and services nationwide without paying full price—wine, food delivery, clothing and more. Enjoy!Claim Your GiftIf wikiHow has helped you, please consider a small contribution to support us in helping more readers like you. We’re committed to providing the world with free how-to resources, and even $1 helps us in our mission.Support wikiHow

    YesNo

    Not Helpful 5Helpful 7

See more answers

Ask a Question

200 characters left

Include your email address to get a message when this question is answered.

Submit

      Advertisem*nt

      Tips

      • Commercial operations can consider soaking wood in anhydrous ammonia. Once the wood is fully saturated, it bends under light pressure and keeps its new shape once dried.[16] Unfortunately, this chemical is extremely caustic and can produce fatal fumes, making it too dangerous for most home projects. You cannot bend wood with household ammonia.[17] Urea is a safer alternative, but it requires precise and lengthy drying and heating stages.

        Thanks

        Helpful0Not Helpful0

      • Remember, the bigger and smoother the curve, the easier it is to bend. Consider changing your design for the project if there are too many small curves, or shape the wood with a router instead of bending it.

        Thanks

        Helpful0Not Helpful0

      Submit a Tip

      All tip submissions are carefully reviewed before being published

      Submit

      Thanks for submitting a tip for review!

      3 Ways to Make Wood Flexible - wikiHow (27)

      Advertisem*nt

      Warnings

      • Splinter warning.

        Thanks

        Helpful20Not Helpful7

      • Knife and other sharp implements involved.

        Thanks

        Helpful11Not Helpful7

      • Power tools involved.

        Thanks

        Helpful7Not Helpful12

      Advertisem*nt

      Things You'll Need

      Laminating

      • Any straight-grained wood
      • Planer
      • High-strength glue
      • Clamps

      Kerfing

      • Table saw
      • Jig (optional)
      • Wood filler (optional)

      Steaming

      • Air-dried or green hardwood to bend
      • 1½" (3.8 cm) hose
      • Plywood to build mold
      • Bandsaw
      • Work table
      • Dowels or brass rods
      • Drill
      • Clamps
      • Bending strap (optional)
      • Thermometer (optional)

      For steam container, choose one:

      • Plywood, silicone sealant, screws
      • ABS pipe
      • 6 mil polyethylene

      For steam, choose one:

      • Electric kettle
      • Large metal container and electric hot plate
      • Wallpaper steamer

      Expert Interview

      Thanks for reading our article! If you’d like to learn more about woodworking, check out our in-depth interview with Garrett Faust.

      More References (8)

      About This Article

      3 Ways to Make Wood Flexible - wikiHow (41)

      Co-authored by:

      Designer & Fabricator of Custom Wood Wall Art & Signs

      This article was co-authored by Garrett Faust. Garrett Faust is a Designer & Fabricator of Custom Wood Wall Art & Signs. He is also the Co-Founder of Uptown Woodworks based in Minneapolis, Minnesota. With over seven years of professional experience, Garrett and co-founder, Harrison, specialize in creating custom wood wall art and signs. They use CNC lasers and routers to cut out or engrave detailed artwork. Garrett received his B.S. in Mechanical Engineering from the University of St. Thomas. This article has been viewed 273,169 times.

      How helpful is this?

      Co-authors: 25

      Updated: July 5, 2023

      Views:273,169

      Categories: Wood

      Article SummaryX

      If you want to make wood flexible, try steaming it in a box. You’ll need to build a sealed box to hold the wood while it’s steaming. Then, place the wood inside the box and heat it with steam for about 1 hour for every inch of thickness. You can use an electric kettle to do this. Once the time is up, bend the wood to your desired shape by clamping it to a curved piece of plywood. Leave the wood in the bending form for 24 hours in a well-ventilated place so it can cool and dry. For tips on how to kerf wood, read on!

      Did this summary help you?

      • Print
      • Send fan mail to authors

      Thanks to all authors for creating a page that has been read 273,169 times.

      Did this article help you?

      3 Ways to Make Wood Flexible - wikiHow (42)

      Advertisem*nt

      I've been deeply immersed in woodworking for years, exploring various methods to bend wood effectively. I've experimented with laminating, steam bending, and kerfing to create different shapes and curves in wood projects. Each technique has its nuances and challenges, and I've learned from trial and error to achieve the desired results.

      Laminating involves creating a form and gluing thin strips of wood together to increase flexibility. It's a method I've used extensively for creating curved elements in furniture and decorative pieces.

      Steam bending, on the other hand, requires constructing a steam box and carefully heating the wood to make it pliable. This method allows for stronger curves but demands meticulous attention to the steaming process and wood selection.

      Kerfing is a quicker approach where I've learned to make precise cuts against the wood grain to enable bending. While it's faster, it's essential to note its limitations regarding the strength of the resulting curve.

      Understanding the properties of different woods is crucial. I've found that certain hardwoods like oak and hackberry are more suitable for bending due to their grain structure and moisture content.

      Each method necessitates specific tools and precautions, from clamps and steam boxes to safety measures when using power tools. It's vital to consider the project's design and the wood's characteristics before choosing a bending technique.

      In essence, these methods offer diverse ways to manipulate wood, but practice, knowledge of wood behavior, and careful execution are fundamental for successful bending projects.

      3 Ways to Make Wood Flexible - wikiHow (2024)
      Top Articles
      Latest Posts
      Article information

      Author: Errol Quitzon

      Last Updated:

      Views: 6083

      Rating: 4.9 / 5 (59 voted)

      Reviews: 90% of readers found this page helpful

      Author information

      Name: Errol Quitzon

      Birthday: 1993-04-02

      Address: 70604 Haley Lane, Port Weldonside, TN 99233-0942

      Phone: +9665282866296

      Job: Product Retail Agent

      Hobby: Computer programming, Horseback riding, Hooping, Dance, Ice skating, Backpacking, Rafting

      Introduction: My name is Errol Quitzon, I am a fair, cute, fancy, clean, attractive, sparkling, kind person who loves writing and wants to share my knowledge and understanding with you.